| Pitting and stress corrosion cracking in a welded stainless steel tube | Microstructure of a high chromium white iron | Leaded brass cracked as a result of overheating during a machining operation. | |||
|
|
|
|||
| Creep fatique failure in a lead/tin solder circuit board connection | Electron beam weld-steel to copper | Macroetched induction hardened alloy steel | |||
|
|
|
|||
| Ductile iron | Defect in painted polymer | Duplex stainless steel weld | |||
|
|
||||
| Duplex stainless steel microstructure | Laser Welded Nitinol Wire | ||||
|
|||||
|